I saw something somewhere (Paul, I thought it was you who posted it) where you cut the glass in squares and skew 2 layers to get one after firing. Ther was an attachment for sizing….anyone else see this and can you copy me on it?
There is a YouTube video “Bead Kiln Demo 2” by Mark Lauckner about fusing #2 1/2 inch square pieces of glass offset by 45 degrees to get round earrings. Unfortunately I don’t know about larger pieces. Hope this helps!