    has anyone ever forgotten to put kiln wash on their texture mold? i was so excited when i got my new mold i forgot to prepare it. is there a way to get the glass off without ruining the mold?

    #12350
    Stephen Richard
    Participant

    You can try inverting the mould on props.  Heat the glass to around 540C – slowly – and the glass may drop off.