    I am firing stemmed glasses (wine glasses).  the stem is bending.  I need to fire at 1100 degrees.

    is there something I can use to support the stem during firing to stop it from bending?

    I know if I fire to 1050 it will not bend, but I need to get to atleast 1100 or more because of a flux  I am putting on. that needs to fire to atleast 1100.

    thanks so much for any suggestions.Smile

    #13475
    Vernelle
    Participant

    Maybe put some fiber paper underneath to stop the bending.