What firing schedule would you recommend for draping glass? I am a newbie and don’t know if I should just use a slump schedule or if there is a special schedule for draping. I am just making a small piece, a business card holder. Thanks.
We drape and slump at the same time. As with any slump, it is a good idea to look at the piece at slumping temperatures to determine when the slump is complete.