    Hi, I am looking for a full fusing schedule for coe 104 sheet glass. the piece is 7 inches by a and a half inch.

    Thanks in advance.

    Rena

    #13038
    wordana
    Participant

    The higher the COE, the lower the full fuse temperature. 104 usually full-fuses at about 1425. You can adjust the firing schedules found on this site accordingly.From what I am seeing the annealing temp is about 965-970 deg f.

     

    Dana W.

     

    Jester’s Baubles Fused Glass Designs

    http://www.jestersbaubles.com

    #13039
    spundini
    Participant

    Thanks for the quick reply. will try it.

    Rena

     