I have glass scraps in a tube, diameter of 1.5″ height of 4″.tube is lined with thin fire paper, can anyone give me a firing schedule for this? Thx
This will give you the information you need.
http://www.bullseyeglass.com/methods-ideas/annealing-thick-slabs.html
You don’t need to worry much about the heat up as the glass is all in pieces. Choose the schedule for one up from the diameter of your tube.
Stephen Richard