I completed my 2nd pattern bar but I obviously didn’t use enough glass to fill out the design. There are glass gaps around the edge of the piece. I am thinking that I could take this piece and fuse it to a single sheet of glass (which is a coordinating color) and then slump into a dish. I don’t want the design to move too much but I don’t know what type of fuse schedule would be appropriate. Help !!! Idea’s ??