Fibre blanket moulds are good for free form moulds. The blanket can be cut into shapes or crumpled. It does not have binders as the papers do, so kiln wash is not necessary. Still, I have always sprinkled alumina hydrate powder over the mould. You can then support the high spots with kiln furniture – existing or custom made.