    Hey everyone! I am wanting to try a drop ring for the first time…and I am looking for hints, tips, advice…a slumping schedule:) I don’t want the glass to end up melted on my kiln floor. Thanks in advance, Kimberly

    #11413
    Anonymous
    Inactive

    Make sure there is enough rim so that the glass doesn’t pull through the hole.



    Paul
    FusedGlass.Org
    Helios Kiln Glass Studio
    PaulTarlow.com

     

    #11414
    davidgustafson
    Participant

    How much rim is needed? Do you have a guideline? (i.e. deeper drops require more rim) What constitutes “more” rim?