    We have always loved the crackle look in pottery as well as Bob Leatherbarrows wonderful glass Recently we have spend time developing a simpler technique to accomplish a similar look in smaller pieces. Posted 3 picrues in my album here (bookie13) so you can have a look.

    We also have some new crackle pieces on our web site.

     

    Barry Kaiser

    http://www.kaiserglass.com

     

     

     

     

    #12403
    crackedglassman
    Participant

    Hi I like your pictures of crackled pendents. How did you do that?

    #12404
    Stephen Richard
    Participant

    I am not trying to be disrespectful, but Barry has spend a lot of time developing the technique. If you want to know you might think about taking a course from him.

    Stephen Richard

    blogs at: http://www.verrier-glass.blogspot.com/ and  http://www.glasstips.blogspot.com/

Viewing 3 posts - 1 through 3 (of 3 total)
  • You must be logged in to reply to this topic.

People Who Like Thisx

Loading...