    It has finally happened to me, after at least 18 years of experience.  When I took my piece from the kiln after a tack fuse (1400 degrees) There was an ugly grey 1/2 ” blob between the yellow and the white background.  is there any way at to get rid of this?  Alternative would be to introduce random 1/2″ dots in various strategic spots to look like I meant them to be there all along!