    I am having trouble annealing a 3″ thick x 18″ x 26″ bullsyeye slab.

    I tried the recomended bullseye schedule with no luck. Tips?

    #13660
    Vital-Spark
    Participant

    You dont say what went wrong. I have tweaked Bullseye schedule using much slower ramps. IN fact for 3″ I used the 6″ schedule. The first 2 seg need to be really slow (Thermal shock) but if its not that I found the longer i annealled the better with transparent. Never done opals so dont know.