Your firing schedule is too
Home › Forums › Glass Fusing › General Fusing Discussion › Working with Metal Inclusions › Your firing schedule is too
June 27, 2011 at 8:53 pm #12119
Participant
Your firing schedule is too fast unless it is a very small piece. You should also include a “bubble squeeze” with inclusions. This is usually done at about 1100 with a hold that depends on the size of the piece.
Keeping the metal shiny can be done by several methods……either coating with boric acid paste, coating with unique clear paint, etc.