You might try putting the

#12269
Vernelle
Participant

You might try putting the mold upside down on two small kiln posts.  Then heat to aroung 300-500 degrees and see if the mold expands enough to release the glass.   Don’t know if it will work with a mold without kiln wash but you have nothing to lose except a little time.