You can try inverting the
Home › Forums › Glass Fusing › General Fusing Discussion › forgot to wash my texture mold › You can try inverting the
December 17, 2011 at 11:21 pm #12350
Participant
You can try inverting the mould on props. Heat the glass to around 540C – slowly – and the glass may drop off.
Stephen Richard