You aren’t alone in your confusion about kiln schedules. There’s a lot information out there that has been passed around and around without anyone really understanding if the information is any good.
If you can post one of the schedules that came with your kiln I’d be glad to take a look at it.
Paul
FusedGlass.Org
Helios Kiln Glass Studio
PaulTarlow.com