Yes – you can “upgrade”.
The easiest way is a stand-alone controller. It has a thermocouple that you insert through a hole in the side of the kiln (easily made). You then plug the controller into the wall and the kiln into the controller.
Orton has one for $350.
http://www.ortonceramic.com/store/product.php?productid=16386&cat=256&page=1
– Paul