Participant
I have had very good success with mica on black (better than transparent), so I’m surprised that it faded. In most of my pieces, the mica has been on clear, and the clear is placed on the black. Here is a blog post where the mica is on TOP of the clear, and it is fired on black.
http://jestersbaubles.blogspot.com/2017/10/rolling-along-with-mica-powders.html
I also have another blog post: :
http://jestersbaubles.blogspot.com/2015/09/studio-tip-working-with-mica.html
I hope you find these helpful.
Best, Dana