Wire
Home › Forums › Glass Fusing › General Fusing Discussion › Wire for hangers › Wire
August 17, 2012 at 3:24 am #12650
Participant
You can find nickle chromium high temp wire at most glass supply places; i.e.,
http://www.delphiglass.com/fusing-supplies/fusing-tools/17-gauge-high-temp-wire
Dana W.