I have flattened every kind of  bottle you can find in my Skutt, using the basic fusing principles.  I clean the glass well and usually soak them in the sink in hot water and soap overnight.  Then remove the labels, sometimes saving the labels for later use on craft projects or reapply to bottle using decopodge (?sp) paste.  I use the firing schedule that I use for 2 or more layers of glass.  They do have a tendency to devit but you can sandblast a design into this.  My instructors have always been game to try anything I came up with so I am not afraid to experiment.  That is where you get some of the neatest items.  Good luck