Wine Bottle Firing Schedule
Home › Forums › Glass Fusing › General Fusing Discussion › Wine bottled, has anyone a firing schedule? › Wine Bottle Firing Schedule
November 1, 2011 at 12:00 am #12289
Participant
600 1100 10
300 1300 30
AFAP 1425 5 to 15
AFAP 1000 10
180 800 0