Will Glassline paint fuse at slumping temperatures?
Home › Forums › Glass Fusing › General Fusing Discussion › Will Glassline paint fuse at slumping temperatures? › Will Glassline paint fuse at slumping temperatures?
July 12, 2013 at 12:11 am #13001
Participant
Thank you for your suggestion, Stephen. I thought this might be the case, and it’s very good to know I will only need to take it to a tack fuse for the second firing. I’ll slow the firing down as this piece is now 1/4″ thick. I’m usually quite patient, but the poor Glassline paint results had me a bit frustrated. Thanks for getting me back on track!
Carrie L.