warped glass
Home › Forums › Glass Fusing › General Fusing Discussion › Fused project warped and broken › warped glass
July 9, 2018 at 2:02 pm #13760
Participant
I think I just solved my own problem. There is just a slight depression on that kiln shelf. It is not level. I think air got trapped under my large piece of glass. I need to flip that shelf over and use the other side. As for the shattered glass–I will make something truly unique out of the remnants.