Volume control
Home › Forums › Glass Fusing › General Fusing Discussion › A different firing programme › Volume control
July 10, 2014 at 6:32 am #13390
Participant
You have a problem of not enough volume, as glass works best at 6 to 7 mm thicnkess. you are working with 4mm. You dont say what the problem with the results of using the Bullseye schedule may be, so further advice is difficult. I would do my tack fuses at around 785-790C
Stephen Richard
blogs at: http://www.verrier-glass.blogspot.com/ and http://www.glasstips.blogspot.com/