Hi Caren –

With a vitrigraph, the glass comes out the bottom of the kiln (into open air). Vitrigraphs are used to make organic “cords” (stringers) of glass.

When you melt the glass onto a shelf, in a kiln, it pools out – this is called a pot melt (or aperture pour). 

Sounds like you did the second – right?