December 28, 2010 at 8:09 pm #11522
Participant
You have identified exactly the variable that will determine whether the enamel burns off or not. You need to keep records of which temperature and soak burned the enamels off and which did not. You of course are subject to the whims of the manufacturer, because they don’t have any interest in whether the enamel is of exactly the same composistion each time.
Stephen Richard
blogs at: http://www.verrier-glass.blogspot.com/ and http://www.glasstips.blogspot.com/