I’m firing two layers of 3mm glass; clear on the bottom, opal and/or streaky on top (I don’t seem to notice any pits when firing with some of the transparent glasses – perhaps they are just harder to see).  My kiln is a Skutt Box 14, with the elements in the top.  The fusing schedule I’m using is as follows:

400/hr to 1150

150/hr to 1250, hold for 60 minutes

400/hr to 1465, hold for 20 minutes

AFAP to 960, hold for 60 minutes

150/hr to 700, shutoff

I’m considering changing the rate on the second segment to 100/hr…