Using the Bullseye deep mold set can work but it isn’t easy. Getting the glass to fall evenly – even with the mold set – is difficult. It requires a large kiln that heats very evenly.
With drop-out vessels it is easier to get an even drop – but cutting the rim (especially on larger pieces) can be challenging.