Using lava cloth for fusing
Home › Forums › Glass Fusing › General Fusing Discussion › Knowledge or comments regarding using Lava cloth for fusing? › Using lava cloth for fusing
May 25, 2013 at 3:48 pm #12933
Participant
I re fired the 2 pieces at full fuse – the very deep bottom texture was not changed. Bottoms still appear somewhat gray in color. Although the texture makes the transparent top look more interesting I don’t like the look on the bottom at all. Don’t think I will use it again except perhaps a small bit for a design if and when I want that texture. Not overall tho.