Use the same schedule as

Home Forums Glass Fusing General Fusing Discussion Float Glass firing Use the same schedule as

#13559
Chichille8
Participant

Use the same schedule as COE96, with a different holding time at the fusion segment. It should be more for a smaller COE, or less for a higher COE.

As you don’t know, probability for a smaller COE is, so I would go with more HOLD time.