Unfortunately, that
Home › Forums › Glass Fusing › General Fusing Discussion › calculation of electricity used per firing › Unfortunately, that
November 30, 2008 at 10:22 pm #10843
Participant
Unfortunately, that calculation will only give you the cost if it was firing full the whole time. As in a AFAP situation. The elements turn on and off all the time during firing and the usage is less than hours x kiln KW capacity.
A meter is truly the only way that works, but as we see it runs about $250+ if the controller doesn’t have that function.
Steve Worcester