The way to have both sides shiny consistently is to go to glass blowing.
Accept that in fusing one side is going to be smoother than the other – except in special circumstances..
If you really don’t want to accept that, then invest in some serious coldworking.
Really, one side rougher than the other is a feature of fused work.