April 23, 2012 at 6:14 pm #12515
Participant
Hi Paul,
Thanks for the advice and the process. I will try the E6000 again since I have not tried the step of putting them together and pulling them apart. I will also start with a fresh tube of glue, since the opened one I have, even though it still flows well, may be “old” and not worth the risk of having to glue multiple times. I glued 22 pendants yesterday using the tutorial instructions from Barry’s website and I had only TWO that held, so I’m going to assume the glue is bad.
I’ll let you know how it works out.
Barb