Try increasing your temp a
Home › Forums › FusedGlass.Org Website Help › Suggestions & Feedback › slumping › Try increasing your temp a
February 14, 2011 at 11:48 am #11905
Participant
Try increasing your temp a little to 1250 or 1260, depending on the glass slumping temp can go all the way to 1300 which I find a little extream for most but 1260 or so works just fine.