March 11, 2009 at 7:06 pm #11182
Participant
When I just use the top elements the middle bubbles no matter how long of a soak time I have. The kiln just seems to get too hot. If I try to adjust by setting the temperature lower the sides don’t fuse enough. Small pieces are ok — it’s just anything over 10″ that’s a problem.
Thanks for the help!
Karen