Tin side of float
Home › Forums › Glass Fusing › General Fusing Discussion › clear glass › Tin side of float
June 3, 2010 at 6:23 am #11632
Participant
Well actually you can fuse float glass on the tin side. If you put the tin on the bottom of each of a two or more layer piece, you will have tin in contact with the air side and it does fuse. If you put tin to tin it will still fuse, but it is a very bad idea, as any further forming of the glass will show tin bloom.
Stephen Richard
blogs at: http://www.verrier-glass.blogspot.com/ and http://www.glasstips.blogspot.com/