I called Paragon. They directed me to do the paper clip test. I followed the directions and determined it was the thermocouple and not the controller board. Ordered a new one, got it yesterday, followed the directions and I am back in the fusing mode today.
Wasn’t too hard. Needed a second pair of hands to help at times but that significant others are for, right?
Happy Holidays Everyone!
Rachel