July 27, 2010 at 12:16 am #11687
Participant
There was a tutorial on this at the Dick Blick web site but I don’t if it is still there some where under teaching. I wasn’t too successful with it. My plant would turn out part white part black. The trick is not to do a full fuse. If you fuse it too much you will end up with a really big air bubble.