The spikes indicate that you

Home Forums Glass Fusing General Fusing Discussion slumping wine bottles problems The spikes indicate that you

#12426
Stephen Richard
Participant

The spikes indicate that you are firing too hot.  Fire at a lower temperature and soak longer.

Stephen Richard

blogs at: http://www.verrier-glass.blogspot.com/ and  http://www.glasstips.blogspot.com/