The firing schedules on this
Home › Forums › Glass Fusing › General Fusing Discussion › Firing Time Schedule › The firing schedules on this
January 24, 2010 at 5:53 pm #11483
Inactive
The firing schedules on this site (under the Tools menu above) all include step-by-step explanations of WHY each segment has the ramp, temp and hold time that it does. Even if you never use the schedules, reading a couple of them will teach you an enormous amount about how to successfully fire glass.
Paul
FusedGlass.Org
Helios Kiln Glass Studio
PaulTarlow.com