The epsom salt never touches

#12947
Anonymous
Inactive

The epsom salt never touches the pump – I don’t recycle water since that also recirculates ground glass which can interfere with a good cut.



Paul
FusedGlass.Org
Helios Kiln Glass Studio
PaulTarlow.com

 