The duller spots touched the
Home › Forums › Glass Fusing › General Fusing Discussion › Super shiney and non -shiney patches on fused piece › The duller spots touched the
April 17, 2014 at 6:40 pm #13322
Participant
The duller spots touched the mold; the shinier spots did not touch the mold.
Dana W.
Jester’s Baubles Fused Glass Designs