Thanks. I did just that – fired some sample pieces. I happened to be doing a slump firing (float) so stuck some samples in. They did indeed change to what I had originally expected.
Still not sure how to work with them as the colours are completely absent pre-firing. It will mean being super organised I guess and not getting them mixed up!
thanks for for your reply – much appreciated.