April 17, 2014 at 10:37 pm #13330
Participant
Yes, the holes are clear. I will try to increase the temp first since the hold is already 35 min.
I’d prefer not using the schedules usually suggested for a brick kiln in my fiber kiln. I know I could use those traditional schedules but that would be a waste of both time and electricity in this kiln so I am hoping someone else has used a fiber kiln and has experience with schedules. I am keeping a log of all firings.
Thanks, katg