Temperatures for enamels

#12861
marV
Participant

I fired my 2nd piece at 1000 – held for 1 minute and it too came out very pale. I had the kiln lid cracked open about 1″ as this piece had red and orange berries and leaves in a band around the edge. One area of the band came out brighter in color – almost good. It was nearest the small peek hole in the kiln. Anyone have any answers? Now I am going to slump these pieces over my star mold. Then I will add color back to them with my Pebco glass paints and fire them in my kitchen oven. I know that works.