Glasstac doesn’t hold terribly well– it’s the product, not you. Use Suave Extra Hold hairspray. Rave also does the trick. A little of the liquid (try the pump bottle) place onto the glass with a coffee stirrer or a toothpick  actually does a remarkable job of holding pieces together. It burns cleanly, is available, and is cheap.