Tack fusing is generally not
Home › Forums › Glass Fusing › General Fusing Discussion › will tack fusing round the edges of an unfused piec of glass, single sheet? › Tack fusing is generally not
July 8, 2011 at 3:12 am #12142
Participant
Tack fusing is generally not hot enough to round the edges. They won’t be razor sharp, but they’ll pretty much have their original shape.
Dana W.