Tack fuse temp and schedule
Home › Forums › Glass Fusing › General Fusing Discussion › Making small cabochons with opalescents pickup kiln paper. › Tack fuse temp and schedule
June 16, 2013 at 10:55 am #12970
Participant
Hi Stephen
They were fired at 790C (1450F) for 10 minutes. A quick look up seems to say rounded tack fuse is about 760C (1400F). Is that the temp you think may work?
I will try this and observe to see result, but what hold is normal for this temp, and what about the devit problem with opals?