Tack fuse/fire polish
Home › Forums › Glass Fusing › General Fusing Discussion › tack fusing schedule › Tack fuse/fire polish
February 22, 2009 at 4:44 pm #11144
Participant
I want to say thank you, Paul, for this simple schedule. Not being particularly experienced in fusing, I’ve played around with all kinds of fusing schedules with 4 or 5 segments and holds, always wondering how the items will look at the end, and jotting down notes in my firing journal. I have several pendants and a small clock piece that require a tack fuse or fire polish. If a particular piece does not have the look I want, then I’ll refire; otherwise, I using this schedule first.