Surface bubbles
Home › Forums › Glass Fusing › General Fusing Discussion › Surface Bubbles on Thick Peices › Surface bubbles
February 22, 2014 at 2:52 am #13268
Participant
Your ramp up to 1250 may be too fast, but others with more experience would know better than me.
You would still want to stick with your existing anneal and cooldown segments, IMO.
Dana W.
Jester’s Baubles Fused Glass Designs